458Win
New member
Finally got around to swaging up some .375 220gr Hollow Points. For cores I used #9 shot swaged solid. These are basically a varmint grenade in a much larger package. On jackets I used cut down .223 military cases (this is a great use for worn out brass!
For some reason I suspect they will NOT be fur friendly!!
This is a original .223 cases, Case cut off, core seated, and point half formed. (got excited to see what the first one looked liked!)
First 28 bullets finished!
Comparison with 223 case and finished bullet, also 50gr .224 bullet formed out of 22LR case.
Finished products. Set on far right is after final Stainless Tumble cleaning..and ready for loading
For some reason I suspect they will NOT be fur friendly!!
This is a original .223 cases, Case cut off, core seated, and point half formed. (got excited to see what the first one looked liked!)
First 28 bullets finished!
Comparison with 223 case and finished bullet, also 50gr .224 bullet formed out of 22LR case.
Finished products. Set on far right is after final Stainless Tumble cleaning..and ready for loading
Last edited: